Tungsten Carbide Flexible Hardfacing Rope – CTC Series (TWD110*50N)

Tungsten Carbide Flexible Hardfacing Rope – CTC Series (TWD110*50N)


TWD110*50N flexible wear-resistant welding rope with irregular cast tungsten carbide (CTC, 2500–3000 HV) and spherical Ni-Cr-B-Si self-fluxing alloy for oxy-acetylene hardfacing.

E-mail: max@tensileweld.com

Phone / WhatsApp / WeChat: +8615066821752


Product Description

Tungsten Carbide Flexible Hardfacing Rope – CTC Series (TWD110*50N) — is produced by extrusion-coating a ductile nickel core wire with irregular cast tungsten carbide (CTC, 2500–3000 HV) and spherical Ni-Cr-B-Si self-fluxing alloy powder. Designed for oxy-acetylene hardfacing (slightly carburizing flame) at ~1050 °C, it delivers smooth fluidity, strong metallurgical wetting, and ≥52 HRC coating hardness.

Product core positioning: High-abrasion oxy-acetylene flexible hardfacing rope featuring sharp, irregular cast tungsten carbide (CTC) particles (50–68% hard phase) for extreme sliding and gouging wear.

Grades & Standard Specifications (TWD110*50N Series)

Grade Diameter (mm) Hard Phase Carbide Mesh Hard Phase Content Matrix Alloy Coating Hardness
TWD110*50N (Series) Φ4, Φ5, Φ6, Φ8 mm Irregular CTC 20–30 / 80–230 mesh 50–65% Ni-Cr-B-Si alloy powder ≥52 HRC
TWD110550N Φ5.0 CTC 20–30 / 80–230 mesh 68% Ni-Cr-B-Si ≥52 HRC
TWD110650N Φ6.0 CTC 20–30 / 80–230 mesh 68% Ni-Cr-B-Si ≥52 HRC
TWD110850N Φ8.0 CTC 20–30 / 80–230 mesh 68% Ni-Cr-B-Si ≥52 HRC
TWD110450N-1 Φ4.0 CTC 20–30 mesh 60% Ni-Cr-B-Si ≥52 HRC
TWD110550N-1 Φ5.0 CTC 20–30 mesh 60% Ni-Cr-B-Si ≥52 HRC
TWD110650N-1 Φ6.0 CTC 20–30 mesh 60% Ni-Cr-B-Si ≥52 HRC
TWD110850N-1 Φ8.0 CTC 20–30 mesh 60% Ni-Cr-B-Si ≥52 HRC

Base Material & Coating Performance (WC Flexible Rope Material)

Parameter Specification
Cast Tungsten Carbide (Ct / Co / Fe / W) Ct: 3.80–4.10%, Co: ≤0.100%, Fe: ≤0.400%, W: Bal., Hardness: 2200±200 HV (up to 2500–3000 HV)
Nickel-Based Alloy Matrix (wt%) C: 0.02–0.40, Cr: 7.00–8.00, Fe: ≤5.0, B: 1.50–1.90, Si: 2.90–3.80, Ni: Bal., Hardness: 40±2 HRC
Bonding Phase / Hard Phase Ratio 40.0% / 45.0% Bonding Phase — 60.0% / 55.0% Hard Phase
Coating Hardness ≥52 HRC (standard range 47.0–52.0+ HRC)
Metal Deposition Density 11.0–12.0 g/cm³
Deposition / Melting Temperature ~1050 °C (Melting Point: 1050.0–1150.0 °C)
Max Service Temperature <700.0 °C

Core Advantages & Features

  • Flexible spool format enables continuous, uninterrupted oxy-acetylene deposition on complex geometries.
  • Irregular cast tungsten carbide (2500–3000 HV) provides aggressive cutting and abrasion resistance.
  • Low deposition temperature (~1050 °C) minimizes base metal dilution and thermal distortion.
  • Note: ‘*’ denotes wire diameter (4, 5, 6, or 8 mm), e.g., TWD110650N is Φ6.0 mm. Custom specs available.

Typical Application Fields

  • Oilfield stabilizer blades and PDC drill bits
  • Concrete mixer blades, slurry pumps, and wear sleeves
  • Coal mine chutes, drill rods, and TBM wear parts
  • Steel sand-mixer scrapers, press guide rails, and chemical/food mixer screws