Tungsten-Rich, Cobalt-Based & Ultra-High Wear Hardfacing Electrodes (D009–D036 / D406–D437 / D707–D948) — covers our highest-performance specialty SMAW hardfacing electrodes: high-tungsten carbide electrodes (D707/D717 with 40–70% W), cobalt-based superalloy electrodes (D802–D852), cold/hot die electrodes (D009–D437), and ultra-high-wear chromium-boron electrodes (D856–D948).
Product core positioning: Extreme-duty specialty hardfacing electrodes for high-temperature cobalt alloy sealing, 70% tungsten carbide wear armor, and 60–66 HRC heavy abrasion.
Chemical Composition (wt%) & Hardness (D009–D948 Series)
| Product | C | Si | Mn | Mo / B | Cr | Co | S / Fe | P / Fe | W | Other | Hardness |
|---|---|---|---|---|---|---|---|---|---|---|---|
| D009 | ≤0.25 | ≤1.00 | 2.00–3.00 | Mo: 2.00–3.00 | B: ≤0.15 | ≤0.15 | S≤0.03 | P≤0.03 | — | V: 5.00–8.00 | HB ≥180 |
| D017 | 0.25–0.35 | 1.00–2.00 | 0.60–1.50 | — | 5.50–7.50 | — | S≤0.04 | P≤0.04 | — | — | HRC ≥53 |
| D027 | ~0.45 | — | — | Mo: ~0.50 | ~5.50 | — | S: ~2.80 | — | — | V: 0.50 | HRC ≥53 |
| D036 | 0.50–0.70 | 0.60–0.80 | — | Mo: 0.60–0.90 | 5.00–6.00 | — | — | — | — | V: ~0.50 | HRC ≥55 |
| D406 | ≤0.5 | ≤2.0 | ≤2.0 | Mo: ≤5.0 | ≤6.0 | ≤12.0 | V: ≤2.0 | — | ≤10.0 | Other≤2.0 | HRC ≈50 |
| D417 | 0.5–0.9 | ≤0.80 | ≤0.60 | Mo: 5.0–9.5 | 3.0–5.0 | — | S≤0.03 | P≤0.04 | 1.0–2.5 | Other≤1.00 | HRC ≥55 |
| D427 | ~0.8 | — | ~13.0 | — | ~11.0 | — | S≤0.030 | P≤0.030 | V: ~2.0 | Ni: ~2.0 | HRC ≤40 |
| D437 | ~0.8 | — | — | — | ~15.0 | — | S≤0.030 | P≤0.030 | V: ~3.0 | Ni: ~4.0 | 40–42 HRC |
| D707 | 1.50–3.00 | ≤4.00 | — | — | — | — | — | — | 40.00–50.00 | — | HRC ≤60 |
| D717 | 1.50–4.00 | ≤4.00 | ≤3.00 | Mo: ≤7.00 | ≤3.00 | — | — | — | 50.00–70.00 | Other≤3.00 | HRC ≥60 |
| D802 | 0.70–1.40 | ≤2.0 | ≤2.0 | — | 25.0–32.0 | Bal. | — | Fe≤5.0 | 3.0–6.0 | Other≤4.0 | HRC ≥40 |
| D812 | 1.0–1.70 | ≤2.0 | ≤2.0 | — | 25.0–32.0 | Bal. | — | Fe≤5.0 | 7.0–10.0 | Other≤4.0 | HRC ≥44 |
| D822 | 1.75–3.0 | ≤2.0 | ≤2.0 | — | 25.0–33.0 | Bal. | — | Fe≤5.0 | 11.0–19.0 | Other≤4.0 | HRC ≥53 |
| D847 | 0.20–0.50 | ≤2.0 | ≤2.0 | — | 23.0–32.0 | Bal. | — | Fe≤5.0 | ≤9.50 | Other≤7.0 | 25–35 HRC |
| D852 | 0.15–0.40 | ≤2.0 | ≤1.50 | Mo: 4.5–6.5 | 24.0–29.0 | Bal. | Fe≤5.0 | S≤0.03 | ≤0.50 | Ni: 2.0–4.0 | 23–28 HRC |
| D856 | 2.00–3.00 | ≤1.50 | — | B: 0.40–2.00 | 15.0–17.0 | — | S≤0.035 | P≤0.035 | 1.20–1.50 | Other≤5.0 | HRC ≥60 |
| D900 | 3.50–5.00 | ≤1.50 | ≤1.00 | — | 28.00–32.00 | — | — | — | — | Other≤8.00 | 60–65 HRC |
| D938 / D948 | 4.00–5.00 | — | — | — | 25.00–28.00 | — | — | — | — | Other: 8.00–13.50 | D938: 58–62 HRC / D948: 62–66 HRC |
Core Advantages & Features
- Cobalt-based D802 / D812 / D822 / D847 / D852 provide exceptional red-hardness, thermal shock, and corrosion resistance up to 800 °C.
- Tungsten carbide electrodes D707 (40–50% W) and D717 (50–70% W) deliver extreme rock and abrasive wear protection.
- D900 / D938 / D948 achieve 60–66 HRC for high-stress mineral crushing and grinding.
Typical Application Fields
- High-temperature petrochemical valves, turbine blades, and engine valve seats (D802–D852)
- Oilfield drill bits, mining cutters, and extreme rock-wear parts (D707 / D717)
- Cold/hot stamping dies, brick-making augers, and cement mill liners (D009–D437, D900–D948)