Stainless Steel Hardfacing Flux-Cored Welding Wires (TW307–TW631N Series) — provides austenitic, martensitic (13Cr / 17Cr), and precipitation-hardening stainless steel flux-cored hardfacing wires engineered for thermal fatigue, corrosion, cavitation, and high-temperature metal-to-metal wear.
Product core positioning: Corrosion- and thermal-fatigue-resistant stainless steel hardfacing FCW family (125 HB to 57 HRC) widely used in metallurgical continuous casting rolls and petrochemical valves.
Part 1: Austenitic & 13Cr Martensitic Series (TW307–TW414N) — Chemical Composition (wt%) & Hardness
| Product | C | Si | Mn | Cr | Ni | Mo | V / Re / Nb | W / Nb / N | Fe | Hardness |
|---|---|---|---|---|---|---|---|---|---|---|
| TW307-G / TW307-S | 0.10 | 0.90 | 7.10 | 17.30 | 8.50 | — | — | — | Bal. | 135–175 HB |
| TW307Mo-S | 0.05 | 0.80 | 4.00 | 20.00 | 9.80 | 1.10 | — | — | Bal. | 135–175 HB |
| TW308L-O | 0.03 | 0.80 | 1.00 | 20.00 | 10.50 | — | — | — | Bal. | 150–180 HB |
| TW309Mo-O | 0.05 | 0.80 | 1.00 | 23.50 | 12.50 | 2.30 | — | — | Bal. | 150–180 HB |
| TW310MnRe-S | 0.12 | 0.30 | 6.50 | 26.80 | 21.30 | — | Re: 0.25 | — | Bal. | 125–175 HB |
| TW310Nb-S | 0.08 | 0.70 | 4.00 | 25.50 | 20.80 | 1.50 | Nb: 0.70 | W: 1.30 | Bal. | 225–275 HB |
| TW316L-O | 0.03 | 0.90 | 0.80 | 19.50 | 12.50 | 2.70 | — | — | Bal. | 125–175 HB |
| TW356-S | 0.70 | 0.65 | 1.25 | 12.00 | 0.70 | 3.80 | V: 2.00 | W: 0.90 | Bal. | 48–52 HRC |
| TW385-S | 1.80 | 0.45 | 1.35 | 16.00 | — | 0.50 | — | — | Bal. | 53–56 HRC |
| TW410L-G | 0.30 | 0.45 | 1.25 | 12.50 | — | — | — | — | Bal. | 225–275 HB |
| TW411L-S | 0.04 | 0.45 | 0.65 | 14.80 | 1.00 | 0.50 | V: 0.05 | Nb: 0.08 | Bal. | 250–300 HB |
| TW411-S | 0.12 | 0.36 | 1.20 | 12.50 | 1.50 | 0.95 | — | — | Bal. | 39–45 HRC |
| TW411N-G / TW411N-S | 0.05 | 0.65 | 1.50 | 12.50 | 1.55 | 0.60 | V: 0.35 | N: 1.70 | Bal. | 35–37 HRC (after 600°C: 39–43 HRC) |
| TW412L-S | 0.07 | 0.36 | 0.09 | 12.50 | 2.40 | 0.81 | V: 1.30 | — | Bal. | 40–45 HRC |
| TW412-S | 0.12 | 0.43 | 0.95 | 12.70 | 2.48 | 0.95 | V: 1.20 | — | Bal. | 45–50 HRC |
| TW413-S | 0.10 | 0.46 | 1.05 | 12.75 | 3.25 | 1.20 | V: 0.21 | Nb: 0.17 | Bal. | 38–42 HRC (after 560°C: 42–45 HRC) |
| TW413N-S | 0.04 | 0.40 | 1.20 | 12.98 | 3.35 | 1.30 | V: 0.08 | Nb: 0.15 | Bal. | 44–50 HRC |
| TW414N-S / TW414N-O | 0.04 | 0.70 | 1.20 | 12.50 | 4.00 | 0.40 | — | N: 0.10 | Bal. | 44–50 HRC |
Part 2: High-Temperature Martensitic & 17-4PH Series (TW415–TW631N) — Chemical Composition (wt%) & Hardness
| Product | C | Si | Mn | Cr | Ni | Mo | V / N / Cu | W / Nb / Co | Fe | Hardness |
|---|---|---|---|---|---|---|---|---|---|---|
| TW415-G / TW415-S | 0.07 | 0.45 | 1.15 | 13.00 | 5.50 | 1.05 | — | — | Bal. | 38–42 HRC (after 520°C: 39–43 HRC) |
| TW415N-S | 0.04 | 0.70 | 1.20 | 12.50 | 3.50 | 1.20 | N: 0.09 | — | Bal. | 43–48 HRC |
| TW416N-S | 0.03 | 0.75 | 1.25 | 12.80 | 1.55 | 0.65 | V: 0.12 | W: 0.75 | Bal. | 37–40 HRC (after 630°C: 40–45 HRC) |
| TW417N-S | 0.03 | 0.80 | 1.20 | 12.80 | 5.00 | 0.60 | V: 0.50 | W: 0.80 | Bal. | 38–40 HRC (after 630°C: 44–50 HRC) |
| TW418N-O / TW418N-S | 0.30 | 0.60 | 1.35 | 12.75 | 5.00 | 1.80 | V: 0.30 | W: 1.05 | Bal. | 40–45 HRC (after 600°C: 44–50 HRC) |
| TW420-S | 0.27 | 0.40 | 1.50 | 13.50 | — | — | — | — | Bal. | 50–55 HRC |
| TW421-S | 0.25 | 0.25 | 0.90 | 12.70 | 0.50 | 1.05 | V: 0.25 | — | Bal. | 49–53 HRC (after 530°C: 45–47 HRC) |
| TW422-S | 0.35 | 0.25 | 1.20 | 12.00 | 1.50 | 0.21 | V: 0.30 | W: 3.50 | Bal. | 55–57 HRC (after 550°C: 50–54 HRC) |
| TW423-S (High-C) | 0.25 | 0.50 | 1.20 | 12.30 | 0.10 | 1.00 | V: 0.17 | Nb: 0.18 | Bal. | 49–51 HRC (after 510°C: 46–48 HRC) |
| TW425-S | 0.27 | 0.60 | 1.20 | 12.80 | 0.60 | 1.80 | V: 0.19 | W: 1.40 | Bal. | 50–55 HRC |
| TW426-S | 0.28 | 0.45 | 1.35 | 12.60 | 0.50 | 1.05 | V: 0.25 | W: 0.80 | Bal. | 50–55 HRC |
| TW429-S | 0.25 | 0.36 | 1.25 | 12.20 | 0.60 | 2.70 | V: 0.25 | Co: 1.50 | Bal. | 49–52 HRC (after 550°C: 46–48 HRC) |
| TW430-S / TW430-G | 0.07 | 0.50 | 1.25 | 18.00 | — | — | — | — | Bal. | 170–200 HB |
| TW430NiMo-S | 0.05 | 0.65 | 1.20 | 17.00 | 5.60 | 1.30 | — | — | Bal. | 150–180 HB |
| TW431-S | 0.40 | 0.90 | 1.00 | 17.00 | 0.50 | 1.10 | — | — | Bal. | 30–35 HRC |
| TW423-S (Low-C) | 0.04 | 0.45 | 0.60 | 19.70 | 4.20 | 1.40 | V: 0.18 | Nb: 0.15 | Bal. | 200–240 HB |
| TW630-S | 0.05 | 0.40 | 1.20 | 16.00 | 5.50 | 0.60 | Cu: 3.00 | Nb: 0.20 | Bal. | 175–225 HB |
| TW630N-S | 0.05 | 0.40 | 1.20 | 16.00 | 5.50 | 0.60 | Cu: 4.00 | Nb: 0.10 | Bal. | 35–39 HRC |
| TW631N-S | 0.05 | 0.40 | 1.20 | 13.00 | 5.50 | 0.60 | Cu: 3.00 | Nb: 0.10 | Bal. | 37–41 HRC |
Core Advantages & Features
- Nitrogen-alloyed martensitic grades (TW414N / TW415N / TW418N) offer exceptional resistance to thermal checking and corrosion.
- Smooth submerged-arc and open-arc slag detachability with low crack sensitivity.
- Retains hardness after tempering up to 600–630 °C.
Typical Application Fields
- Steel mill continuous casting rolls (CCM rolls) and table rolls
- Valve seats, pump shafts, and hydro turbine cavitation repair
- Corrosive high-temperature industrial rollers and steam fittings