Nickel-Based Alloy Hardfacing Flux-Cored Welding Wires (TW920–TW982 Series) — delivers high-nickel superalloy and boron-hardened nickel flux-cored welding wires (gas-shielded -G and submerged-arc -S) for severe corrosion, thermal shock, and high-temperature wear environments.
Product core positioning: Superalloy nickel-based cladding & hardfacing FCW family (150–230 HB corrosion-resistant alloys up to 58–62 HRC wear-resistant NiCrBSi).
Chemical Composition (wt%) & Hardness (TW920–TW982 Series)
| Product | C | Si | Mn | Cr | Nb | Mo | Fe | Ni | Other | Hardness |
|---|---|---|---|---|---|---|---|---|---|---|
| TW982-G (Ni6082) | 0.03 | 0.30 | 3.00 | 20.00 | 2.50 | — | 1.50 | Bal. | — | 175–225 HB |
| TW976-G / TW976-S (Inconel C-276) | 0.05 | 0.35 | 1.30 | 16.00 | 13.80 | — | 3.00 | Bal. | Co: 2.50 | 190–210 HB |
| TW960-G (Ni608A) | 0.75 | 4.50 | 0.20 | 16.20 | — | 2.00 | 4.50 | Bal. | B: 3.10 | 58–62 HRC |
| TW925-G / TW925-S (Inconel 625) | 0.03 | 0.30 | 0.25 | 22.30 | 3.80 | 9.00 | 1.50 | Bal. | — | 150–200 HB |
| TW920-G (Udimet 520) | 0.04 | 0.25 | 0.30 | 19.00 | — | 6.00 | 2.50 | Bal. | Co: 13.00, W: 1.00, Ti: 3.00, Al: 2.00 | 180–230 HB |
Core Advantages & Features
- Superior resistance to high-temperature oxidation, pitting, crevice corrosion, and aggressive chemical media.
- TW960-G (Ni608A) delivers 58–62 HRC wear hardness combined with nickel-matrix corrosion resistance.
- Available in gas-shielded (-G) and submerged-arc (-S) versions for high-deposition industrial cladding.
Typical Application Fields
- Petrochemical reactors, waste-to-energy boiler tubes, and flue-gas desulfurization (FGD) equipment
- High-temperature hot forging dies, valve trim, and corrosive pump components
- Offshore oil & gas subsea equipment cladding