Carbide-Based Thermal Spray Powders – WC-Cr3C2-Ni & Cr3C2-NiCr Series (TWD07N / TWD10NC–TWD58NRU)

Carbide-Based Thermal Spray Powders – WC-Cr3C2-Ni & Cr3C2-NiCr Series (TWD07N / TWD10NC–TWD58NRU)


High-temperature WC-Cr3C2-Ni (up to 750°C) and Cr3C2-NiCr / Cr3C2-CoNiCrAlY (up to 850–1000°C) thermal spray powders for steel furnace rolls, valve stems, and chrome replacement.

E-mail: max@tensileweld.com

Phone / WhatsApp / WeChat: +8615066821752


Product Description

Carbide-Based Thermal Spray Powders – WC-Cr3C2-Ni & Cr3C2-NiCr Series (TWD07N / TWD10NC–TWD58NRU) — is specially engineered for elevated-temperature oxidation, hot gas corrosion, and abrasive wear up to 750–1000 °C, as well as cobalt-free and cost-effective hard chrome plating replacement.

Product core positioning: High-temperature (750–1000 °C) Cr3C2-NiCr and corrosion-resistant WC-Cr3C2-Ni / WC-NiMoCrFeCo HVOF/HVAF thermal spray powder portfolio.

Grades, Compositions, Particle Sizes & Applications

Grade Series Composition Type Available Particle Sizes Properties & Applications
TWD07N-9 / -3 / TWD07N / -2 / -7 / -19 / -16 WC-20Cr3C2-7Ni Agglomerated & Sintered -90/+45, -53/+20, -45/+15, -38/+15, -38/+10, -30/+5, -25/+5 µm HVOF/HVAF. 1. Max service temp: 750°C. 2. Better corrosion & oxidation resistance than WC-Co. 3. High wear & corrosion parts.
TWD06N-3 / TWD06N WC-21Cr3C2-6Ni Agglomerated & Sintered -53/+20 µm, -45/+15 µm HVOF/HVAF. 1. Max service temp: 750°C. 2. Better corrosion & oxidation resistance than WC-Co.
TWD16NR / -19 / -16 WC-19Cr3C2-16Ni Agglomerated & Sintered -45/+15, -30/+5, -25/+5 µm HVOF/HVAF. 1. Max service temp: 750°C. 2. Better corrosion & oxidation resistance than WC-Co. 3. Higher toughness than TWD07N.
TWD11NM / -2 / -20 WC-20Cr3C2-8.5Ni-2.5Mo Agglomerated & Sintered -45/+15, -38/+15, -30/+10 µm HVOF/HVAF. 1. Max service temp: 750°C. 2. Better corrosion resistance than WC-Co. 3. Demanding corrosive environments.
TWD18NM / TWD18NM-2 WC-18(NiMoCrFeCo) Agglomerated & Sintered -45/+15 µm, -38/+15 µm HVOF/HVAF. 1. Max service temp: 500°C. 2. Hastelloy-like high corrosion resistance. 3. Superior corrosion resistance over WC-Co-Cr & WC-Ni.
TWD09CN / TWD10N5C / TWD30N6C WC-9Co-5Cr-1Ni / WC-10Ni-5Cr / WC-30Ni-6Cr Agglomerated & Sintered -90/+45 to -30/+5 µm HVOF. Max service temp: 500°C. Superior saline/pump corrosion resistance & toughness.
TWD10NC / TWD20NC / TWD25NC Series Cr3C2-10/20/25(NiCr) Agglomerated & Sintered -90/+45 down to -20/+5 µm HVOF. 1. Medium-grain Cr3C2. 2. Max service temp: 850°C. 3. Good corrosion & impact resistance. 4. High-temp stability. 5. Steel furnace rolls, valve stems & ball valves.
TWD25CY-3 / TWD25CY / -2 / -7 Cr3C2-25(CoNiCrAlY) Agglomerated & Sintered -53/+20, -45/+15, -38/+15, -38/+10 µm HVOF/HVAF. 1. Medium-grain Cr3C2. 2. Max service temp: 1000°C. 3. Good corrosion & erosion resistance. 4. Excellent high-temp oxidation resistance. 5. Steel furnace rolls.
TWD18NR / TWD37NT Series Cr3C2-37WC-18(NiCrCo) / Cr3C2-7WC-30(NiCr) Agglomerated & Sintered -45/+15, -38/+15, -38/+10, -30/+10, -30/+5 µm HVOF/HVAF. 1. Good corrosion & erosion resistance. 2. Higher hardness than TWD25NC. 3. Hard chrome plating replacement.
TWD58NRU / -20 / -19 WC-42Cr3C2-16Ni Agglomerated & Sintered -45/+15, -30/+10, -30/+5 µm HVOF/HVAF. 1. Fine-grain WC. 2. Max service temp: 750°C. 3. Cost-effective alternative to WC-Co-Cr. 4. Hard chrome plating replacement.

Core Advantages & Features

  • Service temperatures up to 750 °C (WC-Cr3C2-Ni), 850 °C (Cr3C2-NiCr), and 1000 °C (Cr3C2-CoNiCrAlY).
  • Hastelloy-like (TWD18NM) and cobalt-free (TWD58NRU) grades deliver top-tier corrosion protection.
  • Proven, environmentally compliant alternative to electrolytic hard chrome plating.

Typical Application Fields

  • Steel annealing furnace rolls and high-temperature hearth rolls
  • Gas-corrosive valve stems, ball valves, and petrochemical pumps
  • Boiler tubes, gas turbines, and hard chrome plating replacement parts